Powder Coating Troubleshooting: Cloudiness of Coating (Loss of Gloss)

We will also introduce measures to address the issue of the uneven balance between new powder and old powder in the recovery tank!

The phenomenon of the gloss of the coating differing in certain areas or overall is referred to as "cloudiness (loss of gloss) of the coating." Here, we introduce troubleshooting for this issue. If the cause is due to deficiencies in the curing conditions (such as overbaking or gas checking), it is possible to take measures by reconsidering the curing conditions or purifying the atmosphere gas in the curing oven. Additionally, there are measures for issues caused by uneven charging of the coated object. [Causes and Measures (Excerpt)] ■ Due to deficiencies in curing conditions (such as overbaking or gas checking) → Reconsider the curing conditions → Purify the atmosphere gas in the curing oven ■ Because the difference in film thickness is extremely large (especially for matte powder coatings) → Ensure the film thickness recommended by the manufacturer *For more details, please refer to the PDF document or feel free to contact us.

  • paint

Added to bookmarks

Bookmarks list

Bookmark has been removed

Bookmarks list

You can't add any more bookmarks

By registering as a member, you can increase the number of bookmarks you can save and organize them with labels.

Free membership registration

Powder Coating Troubleshooting

We will also introduce measures related to painting over metal powder and debris that have adhered to the coated surface!

We will introduce troubleshooting for the phenomenon known as "butsu," which is characterized by small protrusions that appear on the coating film. If the cause is a blockage in the circulation path (such as the paint hose), it is possible to take measures by preventing the accumulation of powder, heat, humidity, and excess pressure in the paint hose from the recovery tank to the powder coating gun. Additionally, there are measures for cases where aggregated paint forms clumps that fly onto the workpiece and are baked on as is. [Causes and Measures (Excerpt)] ■ Blockage occurred in the circulation path (such as the paint hose) → Prevent the accumulation of powder, heat, humidity, and excess pressure in the paint hose from the recovery tank to the powder coating gun. ■ Aggregated paint formed clumps that flew onto the workpiece and were baked on as is → Remove the powder coating from the box, loosen it while still in the inner bag, and then set it in the painting machine. → Use the "IPD Micronization Powder Coating Control System." *For more details, please refer to the PDF materials or feel free to contact us.

  • paint

Added to bookmarks

Bookmarks list

Bookmark has been removed

Bookmarks list

You can't add any more bookmarks

By registering as a member, you can increase the number of bookmarks you can save and organize them with labels.

Free membership registration