Lithium silicate-based mixed surface impregnation material "Inner Protect"
Suppress alkali-silica reaction (ASR) and prevent internal cracking.
In recent years, there have been reports of cases in Hokkaido where concrete cracking, previously thought to be due to salt damage or freeze damage, was actually caused by alkali-silica reaction. The Inner Protect product from Aimus, when applied to the surface of concrete, penetrates from the surface and generates insoluble gel within the microcracks and voids of the concrete, even at a depth of 40mm. This prevents water intrusion into the concrete's interior, thereby protecting against freeze damage, salt damage, and deterioration of the concrete from within due to alkali-silica reaction.
- Company:日本仮設 本社
- Price:Other