Concrete corrosion protection for water treatment facilities: "Z Mortar KS500 Method"
For the repair and corrosion protection of concrete affected by the erosive action of substances like sulfuric acid in wastewater and waste treatment facilities.
The "Z Mortar KS500 Method" is a corrosion protection method using sulfuric acid-resistant mortar based on blast furnace slag. It complies with the quality standards for sulfuric acid-resistant mortar for protective coatings as specified in the Japan Sewerage Agency's "Manual on Corrosion Control Technology and Protective Technology for Concrete Structures in Sewers." Designed with a concept that allows for a reduction in cross-sectional area, it predicts the amount of reduction in cross-section or the depth of carbonation due to deterioration, setting a reduction amount or carbonation depth that does not pose structural issues. Alternatively, it involves pre-thickening the cross-section and maintaining the facility's functionality through repeated repairs while conducting regular inspections. 【Features】 ■ Exhibits excellent sulfuric acid resistance due to the formulation of special powders based on blast furnace slag. ■ Can be applied in high humidity environments and construction conditions with high moisture content in concrete, which conventional coating lining methods cannot accommodate. ■ Eliminates the need for overlapping processes in coating lining methods, resulting in shorter construction processes and curing periods, thus reducing construction time. ■ Reduces resource and energy consumption, as well as CO2 emissions, by using blast furnace slag. *For more details, please refer to the PDF document or feel free to contact us.
Inquire About This Product
basic information
【Physical Properties and Performance】 <Item: Quality Standards> ■ Compressive Strength (N/mm): Age 28 days 24 or more ■ Adhesion (N/mm): Age 28 days 1.5 or more ■ Length Change Rate (%): Age 28 days -0.1 or more ■ Acid Resistance Weight Change Rate (%): After immersion in 5% sulfuric acid for 112 days ±10 or less ■ Sulfuric Acid Penetration Depth (mm): After immersion in 5% sulfuric acid for 112 days Type B: 10.5 or less, Type C: 6.0 or less *For more details, please refer to the PDF document or feel free to contact us.
Price range
Delivery Time
Applications/Examples of results
【Purpose】 ■Repair and corrosion protection of concrete subjected to sulfuric acid erosion in sewage, wastewater, excrement, and waste treatment facilities. *For more details, please refer to the PDF document or feel free to contact us.
catalog(1)
Download All CatalogsCompany information
The JER Concrete Repair and Improvement Association aims to extend the lifespan and protect concrete structures such as wastewater treatment facilities, pipeline facilities, water supply facilities, agricultural community facilities, irrigation channels, bridges, and dams. We select materials and construction methods that meet our customers' needs and provide high-quality construction. Additionally, we have established a subcommittee within the association called the "Pipeline Subcommittee" to address measures for extending the lifespan of sewer pipeline facilities.