Re-coating is possible multiple times! We also introduce a peeling method that reduces the burden on the substrate.
Fluororesin coatings can be "re-coated" multiple times. When re-coating with fluororesin, it is necessary to first strip the current fluororesin coating. This is done using sandblasting, which inevitably takes a long time. Therefore, for plates under 1mm or precision parts, it is essential to choose a coating that will not affect the substrate even after stripping the fluororesin coating. At Daito Kasei, we also offer processing methods that do not burden the substrate during re-coating. 【Stripping Methods for Each Coating】 ■ Polyurethane Coating - Soak in solvent to strip → Sandblast ■ Ceramic Coating - Clean → Heat treatment → Sandblast ■ Polyethylene Coating - Heat until the surface softens, then strip → Heat treatment → Sandblast *For more details, please refer to the external link page or feel free to contact us.
Inquire About This Product
basic information
【Methods for Stripping Other Coatings】 ■Silicone Coating ・Cleaning → Baking → Sandblasting ■Nickel Plating, Electroless Nickel Plating, Zinc Plating ・Baking → Sandblasting ■Hard Chrome Plating ・After Stripping Plating → Baking → Sandblasting *The above is just one example. Depending on the substrate, different stripping methods may be used. *For more details, please refer to the external link page or feel free to contact us.
Price range
Delivery Time
Applications/Examples of results
For more details, please refer to the external link page or feel free to contact us.
catalog(1)
Download All CatalogsCompany information
It is possible to apply a fluororesin coating (Teflon coating) on the inside of a pipe with an inner diameter of just 1mm. We may be able to handle processing that other companies have declined. Additionally, we have extensive experience in applying coatings for corrosion prevention on manufacturing equipment. We also have a track record in household goods and food-related equipment.