For static electricity trouble prevention! Ω High-performance anti-static silicone roller Ω

【The color tone is gray, and the surface resistivity is 10^6 to 10^8 Ω/□】【Almost no color transfer!】
《The static electricity issues faced by silicone rubber rollers》
Ω: At a conductivity level of 10^4 to 10^5 Ω/□, carbon is often used as a conductor, resulting in a color tone of only black, with frequent color transfer to the workpiece.
Ω: Although white variants are available, their resistivity is high at 10^8 to 10^12 Ω/□.
◆ Our high-performance static electricity prevention silicone rollers solve these static electricity issues with silicone rubber!
《High-performance static electricity prevention silicone rubber》
Ω: Maintains a gray color tone through the use of special conductors!
Ω: Almost no color transfer!
Ω: Surface resistivity is 10^6 to 10^8 Ω/□ (※ in-house test values)
Ω: Molded in a clean room, so there is no concern about foreign matter contamination!
We are also developing hardness below 50°. If you are experiencing static electricity troubles, please feel free to contact us.

Inquiry about this news
Contact Us OnlineMore Details & Registration
Details & Registration
Related Documents
Related Links
If you are viewing our product page from the architectural building materials, interior, or pharmaceutical food technology, we kindly ask you to download from the link "Catalog Download Exclusive Site."